Please log in to reply.
250掳C, 0.2 layer. Fine then sudden under-extrusion. Cold pulls look carbonised.
250掳C, 0.2 layer. Fine then sudden under-extrusion. Cold pulls look carbonised.
Dry the filament, drop speed, add a 1掳C heat-break margin. A worn PTFE tube at the heat break is the usual cause on Bowden.